MEGIA, Pedro J.; MORENO DE LA CALLE, Alvaro; Vizcaíno, Arturo; Calles, Jose A; CARRERO, ALICIA, 2028, "Sustainable hydrogen production from green methanol using agglomerated catalysts: a design-of‑experiments approach", https://doi.org/10.21950/TWMUB1, e-cienciaDatos, V1
This database includes all the data from figures included in the publication: "Sustainable hydrogen production from green methanol using agglomerated catalysts: a design-of‑experiments approach" |
May 21, 2026 -
Sustainable hydrogen production from green methanol using agglomerated catalysts: a design-of‑experiments approach
Tabular Data - 4,1 KB
|
May 21, 2026 -
Sustainable hydrogen production from green methanol using agglomerated catalysts: a design-of‑experiments approach
Texto plano - 8,1 KB -
MD5: 7e4b52313b39b3b048374c064f9a786c
|
May 12, 2026
MORENO DE LA CALLE, Alvaro; Martin-Gamboa, Mario; Calles, Jose A; MEGIA, Pedro J.; Vizcaíno, Arturo; CARRERO, ALICIA, 2028, "Renewable hydrogen from pine wood waste via pyrolysis and autothermal steam reforming: technoeconomic and environmental performance of single and co-production pathways.", https://doi.org/10.21950/XPBQ9Q, e-cienciaDatos, V1
This database includes all the data from figures included in the publication: "Renewable hydrogen from pine wood waste via pyrolysis and autothermal steam reforming: technoeconomic and environmental performance of single and co-production pathways." |
Hoja de cálculo MS Excel - 13,7 KB -
MD5: aec7330b5f134e7a3a549001349f38d1
|
Texto plano - 25,0 KB -
MD5: 21da6b188a93efa8ec4a7648772ed96e
|
May 8, 2026
López Martin, Juan José; MEGIA, Pedro J.; Vizcaíno, Arturo; Calles, Jose A; CARRERO, ALICIA, 2027, "Role of zeolite framework and acidity in Cu-based catalysts for dimethyl ether steam reforming", https://doi.org/10.21950/LGVK31, e-cienciaDatos, V1
This work investigates the influence of zeolite structure and acidity on the performance of 10 wt.% Cu‑based catalysts for dimethyl ether steam reforming (DME-SR). Four commercial zeolites (denoted as HFER (Si/Al = 10), HY‑1 (Si/Al = 40), HY‑2 (Si/Al =2.6) and HZSM‑5 (Si/Al = 45) were evaluated at 400 and 500 ºC. NH3‑TPD showed differences in total... |
May 8, 2026 -
Role of zeolite framework and acidity in Cu-based catalysts for dimethyl ether steam reforming
Tabular Data - 1,2 KB
|
May 8, 2026 -
Role of zeolite framework and acidity in Cu-based catalysts for dimethyl ether steam reforming
Texto plano - 8,3 KB -
MD5: 8ee85ebb63aca8c68bf4deab5009ed27
|
Mar 2, 2026
MORENO DE LA CALLE, Alvaro; MEGIA, Pedro J.; Calles, Jose A; CARRERO, ALICIA; Vizcaíno, Arturo, 2027, "Shaped mesostructured Ni/CeO2 as active catalysts in hydrogen production from acetic acid oxidative steam reforming", https://doi.org/10.21950/DTGWBT, e-cienciaDatos, V2
Oxidative steam reforming (OSR) of acetic acid was carried out using shaped catalysts prepared by combining Ni supported on mesostructured ceria with various clays (kaolinite, sepiolite, attapulgite, and bentonite). Bentonite or attapulgite extrudates calcined with 1°C/min heating rate demonstrated better mechanical resistance. Higher acetic acid c... |